摘要:We report the influence of an Al(2)O(3) shell on the photoluminescence emission of ZnO nanowires. At room temperature, the spectrum of the core-shell nanowires shows a strong reduction of the relative intensity of the green defect emission with respect to the near-band-edge emission. At 5K an increase of the relative intensity of the surface exciton band with respect to the donor-bound exciton emission is observed. Annealing the core-shell nanowires at 500 °C does not increase the green defect luminescence at 5K. We propose a model explaining the spectral changes.